Quick Answer: How Hot Does Kydex Need To Be To Mold?

What is the best thickness for kydex holster?

08”08” Kydex is the standard thickness for OWB holsters.

It is rugged, has aggressive retention, and produces good definition.

The majority of holster makers use this thickness for their OWB holsters and double magazine carriers..

Is Heating kydex toxic?

It is well known that chlorine is one of the few elements that confers good fire properties to a polymer. … The toxicity of building fire emissions from KYDEX® sheet is neither better nor worse than for many other common materials. The most important products in any fire are heat, smoke and carbon monoxide.

Are leather holsters bad for guns?

Although there are some really nice looking leather options for concealed carry, they can be dangerous to use. Over time and use leather becomes softer and more pliable. When you draw your gun from the holster the leather at the top will tend to collapse, making it difficult and dangerous to re-holster your pistol.

Is kydex better than leather?

It really comes down to personal preference which is better. Kydex holsters come out on top when it comes to retention and reholstering. Leather holsters take the crown when it comes to comfort and style. … The best holster is the one you are going to carry everyday.

How durable is kydex?

Relatively hard thermoplastic, with a hardness of 90 on the Rockwell R scale. This hardness, combined with a grained surface, increases its abrasion resistance.

Will hot kydex hurt my gun?

Anything over 350 and the kydex gets a sheen to it. From what I’ve seen, 350 is the sweet spot. I’ve used one gun a few times as the mold. Hasn’t hurt the finish at all, and the gun doesn’t seem to get horribly hot, even after 10-15 minutes in the press.

Will kydex scratch my gun?

Kydex Holsters Leave Marks on My Gun’s Finish. … But the concern towards rub marks is real and can also be found with leather holsters. In fact if a gun is drawn and re-holstered enough times it will leave rub marks on any finish whether it is leather or plastic.

At what temperature does kydex soften?

165 – 177°C( 330 – 350°F ) for 0.71mm – 1.50mm (0.028” to 0.060”). 182 – 196°C (360 – 385°F) for 1.50mm – 3.20mm (0.060” to 0.125”). 65.5ºC (150ºF) before removing the part from the mold.

Can you vacuum form kydex?

Vacuum forming kydex is easy when you have the right tools.

Can kydex be reshaped?

If it is true Kydex and you don’t over heat it, yes it can be heated and reshaped.

Can you heat kydex in the oven?

Preheat oven around 330 deg. put your Kydex in the oven on top of a rock, watch it go limp.. if you got no thermometer just pick it up and if it`s limp like a spaghetti …it`s done…

Can you microwave kydex?

Because kydex doesn’t have water in it, it shouldn’t or won’t work very well and, depending on its resonance frequency, might not heat up at all.

What is the difference between kydex T and kydex V?

KYDEX® T– High impact fire-rated sheet that is less hygroscopic and usually does not require pre-drying. Offers more uniform forming with less wall thinning. … KYDEX® V– Cost-competitive, recycled-grade utility sheet offered only in the color black.

Can you reheat kydex?

Never use an open flame to heat KYDEX® sheet because it will burn. … If a desired shape is not acquired, the KYDEX® sheet may be reheated and reformed for desired results.

Can you heat kydex with a hair dryer?

As with the oven, don’t be tempted to borrow the wifes blow dryer in place of a heat gun. Blow dryers don’t get hot enough, or move enough air to really do a good job with kydex. … If you get a dual mode heat gun, the lower setting will be a lot more forgiving.